Worked walkthrough — Classical Si electronic doping (P/As donors, B acceptors)
- 1 Diagram
- 2 Mechanism
- 3 Failure past the window
- 4 Metastability
- 5 SPECULATIVE Bridge A peg
What’s claimed and how well supported
- Labels on this page
- SPECULATIVE ×13
- Strongest label used
- SPECULATIVE
- Main caveat (quoted)
- Locks: Bridge A locked as ◆ SPECULATIVE supporting case only.
Counted automatically from the labels printed on this page. Counts are a reading aid, not a grade of the page.
Terms on this page (11), plain-language definitions
- Host (matrix)
- Majority element/phase whose lattice dominates the material.
- Dopant
- Intentional dilute impurity meant to tune electronic/optical/catalytic behavior without replacing the host as majority phase.
- Solute
- Intentional minority species dissolved in the host (alloying addition).
- Dislocation
- Line defect enabling plastic slip at realistic stresses; edge vs screw are the two classic geometries.
- Vacancy
- Point defect: a missing atom site in the lattice.
- Valence (chem.)
- Bonding capacity / oxidation-related electron count of an atom in context.
- FCC
- Face-centered cubic — many slip systems; Al, Cu, Ni typically ductile.
- Precipitate
- Second-phase particle that forms (often on aging) and blocks dislocations.
- HCP
- Hexagonal close-packed — fewer primary slip systems; Mg, Ti, Zn often anisotropic.
- BCC
- Body-centered cubic — Fe/steel common; plasticity more temperature-sensitive.
- Valency (ling.)
- Arity: how many actants a predicate takes; formal vs semantic valency can diverge.
Definitions quoted from the Chem for linguists primer glossary.
Materials first. The cross-domain peg stays last, and it stays SPECULATIVE.
Date: 2026-09-19
Audience: syntax/semantics readers building alloy-design literacy (Chem for linguists)
Purpose: Industrial semiconductor electronic-doping baseline — crystalline Si with substitutional group-V donors (P, As) and group-III acceptors (B). Complements Worked examples Example 1 (Si:P) with full checklist discipline matching GaN:Mg / oxide electronic / metal hostsMajority element/phase whose lattice dominates the material.. This is the textbook shallow-dopantIntentional dilute impurity meant to tune electronic/optical/catalytic behavior without replacing the host as majority phase. chassis that oxide research doping and GaN:Mg deep-acceptor doping are measured against.
Locks: Bridge A locked as SPECULATIVE supporting case only. Materials facts first; linguistic parallels only in a flagged box at the end. No joint-field claim. Navajo typed-participant half = light parallel only — not proof of Bridge A count. Dowty / Triskelion / Merge·Agree / kanji not advanced here.
Companion notes: Physics of doping §1–2 (host, dopant, n/p, concentration regimes, T slices); Worked examples Example 1 Si:P; GaN:Mg; Oxide electronic; Conclusions; Grant metal-doping-takeaway.txt §§2–3, 8–9; doping-materials-science-takeaway.txt.
- 0. Design brief (problem-driven)
- 1. Chem-for-linguists checklist (§8) — filled (Si electronic-doping edition)
- 2. Host and dopant cast (REAL materials)
- 3. Concentration windows — under / useful / heavy / over
- 4. Temperature regimes (same sample)
- 5. Process routes (industrial baseline)
- 6. “Over” is plural (name which failure)
- 7. Hard contrast — Si vs GaN:Mg, oxide electronic, metal SSS
- 8. Bridge A add-on checklist (depth note §6) — filled
- 9. Under / useful / over — materials only (no linguistics yet)
- 10. SPECULATIVE Bridge A overlay (supporting only)
- 11. Host contrast card (add Si to the peg set)
- 12. What this walkthrough trains you to do next
- 13. Non-claims
- This walkthrough does not revise Bridge A’s lock, invent shared formalism, or announce a product.
- 14. Sources consulted (2026-09-19 note)
0. Design brief (problem-driven)
| Slot | Choice |
|---|---|
| Host | Crystalline Si (diamond cubic, group-IV; E_g ~1.12 eV at 300 K) |
| Dopants (n-type) | P, As (also Sb) on Si sites — substitutional donors |
| Dopants (p-type) | B (also Al, Ga, In historically) on Si sites — substitutional acceptors |
| Named weakness of pure / intrinsic Si | Intrinsic carrier density n_i ~10¹⁰ cm⁻³ at 300 K — far too low / uncontrolled for transistors, diodes, ICs; conductivity and carrier type must be engineered |
| Intended mechanism | Classical electronic doping — shallow substitutional donors/acceptors → majority electrons (n) or holes (p) at device temperatures |
| Service hint | CMOS / bipolar ICs, power devices, solar cells, sensors — the industrial semiconductor baseline |
Vocabulary lock: here “dopant” is unequivocally correct — intentional dilute impurity for carrier type and density. Same honesty as GaN:Mg and oxide electronic notes; opposite of Al–Mg SSS / Fe–C / Ni–γ′ (prefer soluteIntentional minority species dissolved in the host (alloying addition). / alloying). Grant takeaway + Physics of doping treat Si:B / Si:P as the classical reference.
1. Chem-for-linguists checklist (§8) — filled (Si electronic-doping edition)
1. What is the inherent weakness of the pure / base form?
- Intrinsic Si at 300 K: n = p = n_i ~10¹⁰ cm⁻³ — conductivity too low and not typed for bipolar / FET design.
- Residual unintentional impurities (O from Czochralski, C, metals) can swamp intended doping if the useful window is not engineered.
- Not the weakness: soft yield strength / dislocationLine defect enabling plastic slip at realistic stresses; edge vs screw are the two classic geometries. mobility (that was Al, Mg metal hosts). Different design problem → carrier engineering.
2. Which obstacle / tuning mechanism is doing the work?
Primary: substitutional shallow donors (P, As on Si) → electrons; substitutional shallow acceptors (B on Si) → holes.
Process co-actors (first-class):
1. Ion implantation + anneal — modern device patterning; implant places dose/depth; anneal repairs damage and activates substitutional sites.
2. Thermal diffusion — historical / still used for deep wells / emitters.
3. Czochralski (CZ) melt doping — bulk wafer resistivity set by adding B/P/As to the melt.
4. Compensation — intentional or residual opposite-type impurities set net doping |N_D − N_A|.
Explicitly not: Labusch SSS; oxygen-vacancyPoint defect: a missing atom site in the lattice. photocatalysis; intercalation CT; GaN Mg–H passivation as the headline (Si shallow dopants do not need that story at 300 K).
3. What trade-offs are accepted?
- Higher |N_D − N_A| for lower resistivity / higher drive current ↔ ionized-impurity scattering → mobility drop; bandgap narrowing; eventual impurity-band / Mott MIT.
- Shallow junctions (As) ↔ implant damage / transient-enhanced diffusion (esp. B).
- Heavy CZ doping for low-ρ substrates ↔ constitutional supercooling / growth instability above ~10²⁰ cm⁻³ class.
- Incomplete ionization near Mott densities (device-sim nuance) ↔ often neglected far below / far above N_crit.
4. How critical is processing vs nominal composition?
Extremely — but standardized. Same SIMS [P] can be interstitial/inactive, clustered, compensated, or fully substitutional-activated — depending on implant energy/dose, anneal T/time (RTA spike vs soak), and co-implants (e.g. F with B). Unlike research oxide photocatalysis, Si doping has SEMI / fab process control (Grant takeaway §9 maturity contrast). Characterization (SIMS, SRP, Hall, CV) remains non-negotiable.
5. Problem-driven or exploratory?
Problem-driven and fully industrial. Transistor / IC industry is built on Si:B / Si:P / Si:As. This is the maturity ceiling Grant’s takeaway contrasts with research oxide doping.
2. Host and dopant cast (REAL materials)
2.1 Si host + shallow donors / acceptors
| Item | Approximate figure / fact | Role |
|---|---|---|
| Host | Diamond-cubic Si; E_g ~1.12 eV (300 K); n_i ~10¹⁰ cm⁻³ | Group-IV electronic chassis |
| Donors | P (E_C − E_D ≈ 45.5 meV); As (≈ 53–54 meV); Sb similar | Substitutional n-type → electrons |
| Acceptors | B (E_A − E_V ≈ 44–45 meV) | Substitutional p-type → holes |
| Hydrogenic picture | Binding scaled by m*/(m_e ε_r²); Bohr radius enlarged → shallow levels; ~fully ionized at 300 K in dilute extrinsic window | Contrast vs GaN:Mg (~135–200 meV) |
| Useful device windows | Often ~10¹⁵–10¹⁸ cm⁻³ net doping (channel / well / epi class; process-dependent) | Extrinsic, typically still non-degenerate |
| Heavy / degenerate | Approaching ~N_C, N_V (~10¹⁹ cm⁻³ class at 300 K); source/drain / poly / contact doping often 10¹⁹–10²⁰+ | Impurity band; Fermi–Dirac; Mott MIT |
| Mott N_crit (order) | Si:P ~3.7×10¹⁸ cm⁻³; Si:As ~8.5–8.6×10¹⁸; Si:B ~4×10¹⁸ class | Impurity-state overlap → metallic impurity band |
| Incomplete ionization | Near Mott: up to ~25% P/B, ~35% As non-ionized at 300 K in some models; negligible far below / far above N_crit | Device-sim nuance (Schenk lineage) |
Mechanisms to name:
1. Donor / acceptor substitution — valenceBonding capacity / oxidation-related electron count of an atom in context. excess (P, As) or deficit (B) vs Si → free carriers when ionized.
2. Net doping / compensation — n ≈ N_D − N_A (n-type extrinsic) or p ≈ N_A − N_D (p-type).
3. Implant damage + anneal activation — lattice must be repaired for substitutional electrical activity.
4. Impurity-band / Mott crossover — at high N, discrete H-like levels merge.
5. Clustering / precipitation / mobility collapse — past solubility / stability → inactive aggregates, scattering.
Sources (headline): Ashcroft–Mermin / Sze device framing; Chenming Hu Modern Semiconductor Devices ionization table (~45–54 meV); Delft Open Solid State Notes “Doping and devices”; Schenk incomplete-ionization / Mott N_crit (Si:P 3.74×10¹⁸); Si:As MIT n_c ~8.55–8.60×10¹⁸ (PRB 40, 1216); Physics of doping §1–2; Grant takeaways §§2–3, 8–9.
2.2 Industrial maturity vs GaN:Mg and research oxides
| Aspect | Si:P/As/B | GaN:Mg | Oxide electronic (TiO₂:Fe, AZO) |
|---|---|---|---|
| Maturity | Fully industrial — CMOS / IC fabs (SEMI) | Industrial LED/laser / GaN fabs | Mixed; photocatalysis often research |
| Ionization at 300 K | Shallow → ~full in useful window | Deep → p ≪ [Mg] | Mid-gap / V_O — not H-like shallow |
| Process headline | Implant + RTA; CZ melt doping; diffusion | MOCVD + H depassivation anneal | Synthesis p(O₂) / anneal; ALD/sol-gel |
| Metrology | SIMS, SRP, Hall, CV, sheet ρ | SIMS, Hall, PL, TEM (PIDs) | XRD/XPS/EPR/Hall/PL |
| Grant takeaway | Classical SC baseline | Explicit industrial Mg LED case | Research oxide landscape |
3. Concentration windows — under / useful / heavy / over
| Zone | Si:P / Si:As / Si:B reading |
|---|---|
| Too little | Net doping ≲ mid-10¹⁴–low-10¹⁵ cm⁻³ class (context-dependent) → effect swamped by n_i / residual impurities; “too little → no effect” (Grant §9) |
| Useful / extrinsic window | Often ~10¹⁵–10¹⁸ cm⁻³ — |
| Heavy / degenerate | ~10¹⁹+ cm⁻³ — approaches N_C/N_V; impurity band; Maxwell–Boltzmann fails; Mott MIT near N_crit ~few×10¹⁸ |
| Over / aggregation | Above solubility / stability: dopant clusters, secondary phases, compensation rise, mobility collapse; CZ constitutional supercooling ≳~10²⁰ cm⁻³ |
| Honest split | Degenerate statistics ≠ phase segregation — related high-concentration phenomena, different physics (Physics of doping open Q #7) |
Anchors (not design specs): Physics of doping §2 ladder; worked-examples Si:P column; Schenk Mott N_crit; CZ heavy-doping resistivity windows (B ~0.5–20 mΩ·cm; P ~1–12; As ~2–10 class) with instability above ~10²⁰.
4. Temperature regimes (same sample)
| Regime | Physics (n-type example) | Practical note |
|---|---|---|
| Intrinsic | High T: n_i ≫ | N_D−N_A |
| Extrinsic plateau | Intermediate T: donors fully ionized; n ≈ N_D − N_A (≈ constant vs T) | Room-temperature device window for shallow Si dopants |
| Freeze-out | Low T: k_B T ≪ ionization energy → carriers return to donor/acceptor levels | Cryogenic / physics measurements; hopping near Mott insulator side |
Contrast vs GaN:Mg: Si shallow levels (~45 meV) → room-T ionization is the default; GaN:Mg (~135–200 meV) never reaches that “fully ionized extrinsic plateau” comfort at 300 K.
5. Process routes (industrial baseline)
| Route | What it does | Industrial note |
|---|---|---|
| Ion implant + anneal | Accelerated ions place dose/depth profile; RTA / spike / soak (~900–1050 °C class historically; ms anneals for modern junctions) activates substitutional sites and repairs damage | CMOS default for S/D, wells, VT adjust; As preferred for shallow n+; B harder (TED, clustering) |
| Thermal diffusion | Drive-in from surface source / predep | Deep junctions, older processes, some power devices |
| Czochralski melt doping | B/P/As added to Si melt → bulk wafer resistivity | Substrate / epi starting material; heavy doping limited by constitutional supercooling |
| Epitaxy | In-situ doped epi layers | Precise profiles without implant damage |
Three clocks still apply (Process metastability): equilibrium solubility vs process capture (implant metastable profiles, rapid anneal) vs service (diffusion under later thermal budgets, electromigration-adjacent concerns in metallization — separate from doping itself).
6. “Over” is plural (name which failure)
| Overrun mode | Physics | Where it shows up |
|---|---|---|
| Impurity band / Mott MIT | Wavefunction overlap; discrete levels merge; metallic impurity conduction | Near N_crit ~few×10¹⁸; heavy S/D doping |
| Degenerate statistics | E_F enters band; Fermi–Dirac required | n, p ≳ N_C, N_V (~10¹⁹ class) |
| Clustering / precipitation | Dopant–dopant aggregates; inactive fraction | High dose B clusters; As clustering; post-anneal |
| Mobility collapse | Ionized + neutral impurity scattering; defect density | Hall μ falls with N; conductivity may not keep rising |
| Compensation | Opposite-type impurities cancel net carriers | Intentional counter-doping; residual contamination; implant damage-related defects |
| Incomplete ionization (near Mott) | Bound fraction peaks near N_crit then vanishes above | Device-sim correction; not “failed doping” |
| CZ growth instability | Constitutional supercooling at ≳~10²⁰ | Heavily doped wafer growth limits |
| Implant damage not annealed | Amorphous / defected Si; inactive dopants | Under-annealed process — process failure, not solubility “over” |
Hard contrast vs prior hosts: Al–Mg “over” = GB β; Fe–C = cementite/morphology; oxide electronic = recombination / μ / secondary oxides; GaN:Mg = self-compensation / PIDs / H passivation. Here “over” is electronic MIT + clustering + μ on the most mature fab chassis.
7. Hard contrast — Si vs GaN:Mg, oxide electronic, metal SSS
| Case | Prefer saying | Mechanism | Maturity | Window character |
|---|---|---|---|---|
| This file: Si:P/As/B | Dopant / doping | Shallow subst. donor/acceptor (~45–54 meV) | Fully standardized (SEMI / CMOS) | ~10¹⁵–10¹⁸ useful; ~10¹⁹+ heavy; Mott ~few×10¹⁸ |
| GaN:Mg | Dopant / p-type doping | Deep acceptor + H activation | Industrial LEDs/lasers | [Mg]~10¹⁹; p~10¹⁷; self-comp past peak |
| Oxide electronic (TiO₂:Fe, AZO) | Dopant | Mid-gap / V_O / TCO donors | Mixed; photo often research | at.% class; recombination / μ collapse |
| Al–Mg SSS | Solute / alloying | Dislocation pinning | Industrial alloys | wt% Mg; GB β overrun |
| CNT intercalation | Intercalant | Non-covalent CT in channels | Emerging / specialty | Loading vs moisture / damage |
False-friend reminder: Si shallow doping is the reference electronic-doping story. Do not export its formulas unchanged to TiO₂:Fe (Physics of doping open Q #6) or assume GaN:Mg ionizes like Si:B. Do not call Al–Mg SSS “doped.”
8. Bridge A add-on checklist (depth note §6) — filled
-
Where is the solubility / activation limit at process conditions?
Device windows ~10¹⁵–10¹⁸; heavy doping ~10¹⁹+ with Mott crossover ~few×10¹⁸; CZ / implant solubility ceilings near ~10²⁰ class with clustering. Electrical activation after anneal is the practical limit, not just melt solubility. -
Intended mechanism?
Electronic doping — n/p carriers via shallow substitutional dopants. Name IC / transistor / diode goal. Do not call Al–Mg SSS “doped.” -
What fails first past the window?
Goal-dependent: μ collapse and impurity-band / degeneracy for contacts; clustering / inactive fraction; compensation; CZ growth instability for wafers. -
Metastability?
Yes — as-implanted profiles are non-equilibrium; anneal activates and redistributes; later thermal budgets move dopants (TED for B). Three clocks apply. -
Only then — SPECULATIVE Bridge A mnemonic
See §9. Never invert: do not pick cm⁻³ from a linguistic arity table.
9. Under / useful / over — materials only (no linguistics yet)
| Zone | Si electronic-doping reading |
|---|---|
| Under | Net doping too low; swamped by n_i / residuals; no useful extrinsic control |
| Useful window | ~10¹⁵–10¹⁸ cm⁻³ class extrinsic doping; shallow levels ionized at 300 K; host lattice retained as majority phase |
| Over / wrong regime | Impurity band / Mott MIT; clustering; μ collapse; compensation; CZ instability — name which |
Honest split (repeat): Mott / impurity-band electronic crossover ≠ second-phase solvus overrun. Both can appear at high concentration; they are different physics (Solubility windows §3; Physics of doping open Q #7).
SPECULATIVE Cross-domain section. Open after the materials.
10. SPECULATIVE Bridge A overlay (supporting only)
Everything in this section is pedagogical analogy. It does not make doping × θ-roles a joint field.
Why this host is the textbook electronic Bridge A case: Worked examples Example 1 already used Si:P as the clean underfill → useful window → overfill physics story. Unlike research TiO₂ photocatalyst doping or deep GaN:Mg acceptors, Si shallow doping is the materials community’s default meaning of “dopant,” the industrial maturity ceiling (Grant §9), and the clearest continuous concentration-window ladder for teaching Bridge A’s count intuition — after the materials facts, and only as SPECULATIVE pedagogy.
| Materials fact | SPECULATIVE Bridge A reading |
|---|---|
| Useful ~10¹⁵–10¹⁸ cm⁻³ extrinsic doping | Saturated intended electronic configuration for device regions |
| Intrinsic / under-doped Si | Under-filling relative to typed-carrier design intent |
| Excess → impurity band / Mott / clustering / μ collapse | Overrun / failed regime: “extra” participants force regime repair (overlap, aggregates, compensation) that misses clean extrinsic behavior |
| Continuous N (cm⁻³) vs discrete lexical arity | Asymmetry: concentration is continuous; verb arity is typically discrete — do not force integer slots onto doping curves (Worked examples collapse criterion #1) |
| Donor vs acceptor vs compensator as distinct cast members | Do not smash into one “argument” type |
| Degeneracy ≠ clustering | Do not collapse both into one “over-arity” label (Worked examples collapse #3) |
Earn: helps a linguist remember why Si is the reference electronic-doping window story, why “more dopant” can mean impurity-band / μ loss rather than “more carriers forever,” and why process (implant+anneal) belongs on the doping page.
Collapse: if electrons/holes/vacancies are counted as interchangeable “arguments” without typology; if Mott N_crit is treated as an arity integer; if Si formulas are silently exported to oxide mid-gap systems; if Navajo morphological typing is treated as evidence for this count story; if a joint field is announced.
Navajo typed-participant half — parallel only (not proof)
Navajo morphology saturates typed participants on the verb. Bridge A is the count/windows half. Si doping’s cast (host lattice, donor, acceptor, electron, hole, compensator, anneal process) is a tempting typed-participant mnemonic — keep it parallel, never as evidence that Bridge A’s under/useful/over ladder is proven by Athabaskan morphosyntax.
11. Host contrast card (add Si to the peg set)
| Host | Diagram / lattice | First “over” (typical) | Bridge A peg ( SPECULATIVE) |
|---|---|---|---|
| Al–Mg AA5083 | Limited solvus; FCCFace-centered cubic — many slip systems; Al, Cu, Ni typically ductile. Al + subst. Mg | GB β / sensitization | Solvus overrun → unwanted second phase |
| Cu–Ni | Isomorphous complete SSS | Conductivity / TCR curves | Property-curve overrun |
| Fe–C | Eutectoid Fe–Fe₃C; interstitial C | Cementite / martensite morphology | Transformation / morphology overrun |
| Ni–γ′ | γ/γ′ solvus; wanted precipitateSecond-phase particle that forms (often on aging) and blocks dislocations. | Overaging / TCP | Wanted γ′ vs wrong second phase |
| Mg (host) | HCPHexagonal close-packed — fewer primary slip systems; Mg, Ti, Zn often anisotropic.; AZ/AM/ZK | Brittle IMCs; galvanic β; ignition | β ambivalent; safety “over” |
| Ti (host) | HCP α / BCCBody-centered cubic — Fe/steel common; plasticity more temperature-sensitive. β; β-transus | α-case; ω; O/H embrittlement | Wanted α vs unwanted ω / α-case |
| Oxide electronic | Wide-gap oxide + subst. metal + V_O | Recombination; μ collapse; secondary oxides | Carrier / mid-gap window — true dopant (research-leaning) |
| CNT/graphene intercalation | sp² + guest in channels/gaps | Moisture dedoping; junction R | Intercalant loading window |
| GaN:Mg | III–V wurtzite + Mg_Ga (+ H) | Self-compensation; PIDs; μ/optical loss | Carrier window on industrial deep-acceptor doping |
| Si:P/As/B (this file) | Diamond Si + shallow subst. donors/acceptors | Impurity band / Mott; clustering; μ collapse; compensation | Carrier window on textbook classical electronic doping — true dopant |
12. What this walkthrough trains you to do next
For any classical group-IV / shallow-dopant pair:
- Name the goal (n/p region, well, S/D, substrate resistivity).
- Name donor vs acceptor and net |N_D−N_A| (compensation) separately.
- Sketch under → extrinsic useful → heavy/Mott → clustering — find the device window, not max dissolve.
- Name the process route (implant+anneal / diffusion / CZ) and its activation constraints.
- Name the first failure past the window (μ vs Mott vs cluster vs compensation).
- Only then, if useful for memory, hang the SPECULATIVE Bridge A count peg.
Contrast vs GaN:Mg note: same “dopant” honesty; depth flip — Si is shallow + fully industrial CMOS baseline; GaN:Mg is deep + H-activated LED industrial. Contrast vs oxide note: maturity flip — Si is the ceiling; TiO₂ photocatalysis remains research-grade for many hosts.
13. Non-claims
- No joint field of doping × θ-roles / valencyArity: how many actants a predicate takes; formal vs semantic valency can diverge..
- Bridge A remains SPECULATIVE pedagogy / probe; lock unrevised.
- Navajo θ-morphology does not prove Bridge A count.
- Numbers herein are order-of-magnitude literature / textbook anchors, not fab recipes or process specs.
-
This walkthrough does not revise Bridge A’s lock, invent shared formalism, or announce a product.
14. Sources consulted (2026-09-19 note)
| Source | Role |
|---|---|
Grant metal-doping-takeaway.txt §§2–3, 8–9; doping-materials-science-takeaway.txt; Physics of doping §1–2; grant-doping-cast.md (not published here) |
Project cast; classical SC baseline; concentration ladder |
| Worked examples Example 1 Si:P | Prior Bridge A stress-test column (facts + SPECULATIVE map) |
| Chenming Hu Modern Semiconductor Devices Ch. 1 (ionization ~45–54 meV) | Shallow donor/acceptor energies |
| Delft Open Solid State Notes — “Doping and devices” | Hydrogenic model; extrinsic/intrinsic/freeze-out; impurity-overlap bound |
| Schenk incomplete-ionization model (SISPAD / ETH notes) | Mott N_crit Si:P ~3.74×10¹⁸; ii near Mott |
| Phys. Rev. B 40, 1216 (1989) Si:As MIT | n_c ~8.55–8.60×10¹⁸ |
| Acta Phys. Pol. A 124, 219 CZ constitutional supercooling | Heavy CZ doping limits ≳~10²⁰; B/P/As resistivity windows |
| Implant + RTA activation literature (Mokhberi/Plummer lineage; MIT boron activation models) | Process co-actors |
| Project-internal: GaN:Mg + oxide electronic + CNT intercalation + metal host checklists; CONCLUSIONS-v0 + v1-addendum; chem-for-linguists; depth-solubility-windows; depth-process-metastability | Checklist discipline + contrast |
v0 — 2026-09-19 continue-research. Classical Si electronic-doping industrial baseline walkthrough; Bridge A flagged SPECULATIVE. No joint field.
Corpus note: worked-si-doping-checklist-v0.md. Materials first; Bridge A peg last.