Worked walkthrough — Ni-superalloy γ′ (gamma-prime) precipitation window through the alloy-design checklist
- 1 Diagram
- 2 Mechanism
- 3 Failure past the window
- 4 Metastability
- 5 SPECULATIVE Bridge A peg
What’s claimed and how well supported
- Labels on this page
- SPECULATIVE ×9
- Strongest label used
- SPECULATIVE
- Main caveat (quoted)
- Locks: Bridge A locked as ◆ SPECULATIVE supporting case only.
Counted automatically from the labels printed on this page. Counts are a reading aid, not a grade of the page.
Terms on this page (7), plain-language definitions
- Host (matrix)
- Majority element/phase whose lattice dominates the material.
- FCC
- Face-centered cubic — many slip systems; Al, Cu, Ni typically ductile.
- Precipitate
- Second-phase particle that forms (often on aging) and blocks dislocations.
- Dopant
- Intentional dilute impurity meant to tune electronic/optical/catalytic behavior without replacing the host as majority phase.
- Dislocation
- Line defect enabling plastic slip at realistic stresses; edge vs screw are the two classic geometries.
- Solid solution
- Solute atoms dissolved into the host lattice (substitutional or interstitial) without a separate precipitate phase.
- Solute
- Intentional minority species dissolved in the host (alloying addition).
Definitions quoted from the Chem for linguists primer glossary.
Materials first. The cross-domain peg stays last, and it stays SPECULATIVE.
Date: 2026-09-15 (post-CONCLUSIONS continue-research; after Fe–C)
Audience: syntax/semantics readers building alloy-design literacy (Chem for linguists)
Purpose: Execute the remaining MAIN hostMajority element/phase whose lattice dominates the material. walkthrough named in Conclusions §7: a Ni-superalloy γ′ precipitation window with the same checklist discipline as Al–Mg, Cu–Ni, and Fe–C.
Locks: Bridge A locked as SPECULATIVE supporting case only. Materials facts first; linguistic parallels only in a flagged box. No joint-field claim. Dowty / Triskelion / Merge·Agree / kanji / Navajo θ-typing not advanced here.
Companion notes: Solubility windows; Al / Cu / Fe–C worked checklists; Chem for linguists §4 (precipitation hardening) + §5–§8; Conclusions §3–§4, §7.
- 0. Design brief (problem-driven)
- 1. Chem-for-linguists checklist (§8) — filled
- 2. Explicit phase / diagram reading (diagram first)
- 3. Goal-dependent windows — name the mechanisms
- 4. What “over” means — not one physics
- 5. Metastability / kinetics — first-class
- 6. Vocabulary hygiene
- 7. Bridge A add-on checklist (depth note §6) — filled
- 8. Under / useful / over — materials only (no linguistics yet)
- 9. SPECULATIVE Bridge A overlay (supporting only)
- 10. Contrast table — Ni–γ′ vs Al–Mg vs Cu–Ni vs Fe–C
- 11. What this walkthrough trains you to do next
- 12. Sources consulted (2026-09-15 note)
0. Design brief (problem-driven)
| Slot | Choice |
|---|---|
| Host | Nickel (FCCFace-centered cubic — many slip systems; Al, Cu, Ni typically ductile. γ matrix) |
| Candidate alloy family | Ni-base superalloys strengthened by coherent γ′ — L1₂ Ni₃(Al,Ti) (and related) precipitatesSecond-phase particle that forms (often on aging) and blocks dislocations. in γ; commercial stack includes disk alloys (e.g. Waspaloy / René-class) and blade / SX alloys (high γ′ fraction) |
| Named weakness of pure Ni | Soft / creep-prone at high homologous T; pure Ni lacks the ordered-precipitate obstacle network and the Cr/Al oxidation chemistry needed for hot-section duty |
| Intended mechanism | Precipitation hardening (age hardening) by controlled γ′ size / spacing / volume fraction (+ solid-solution strengtheners in γ; carbides / GB chemistry in polycrystals). Not the Al–Mg SSS-only story; not Fe–C quench martensite; not semiconductor electronic doping |
| Service hint | Aeroengine / gas-turbine hot section: creep strength at high T, plus oxidation / environmental resistance (often with coatings on blades) |
Words like “doped nickel” are avoided for structural superalloys — Al/Ti (etc.) are γ′-formers / alloying additions. Reserve “dopantIntentional dilute impurity meant to tune electronic/optical/catalytic behavior without replacing the host as majority phase.” for dilute electronic (etc.) intent unless a paper’s electronic goal is explicit.
Hard contrast to prior checklists: Al–Mg and Cu–Ni headline solid-solution windows; Fe–C headlines interstitial C + transformation paths. Ni–γ′ headlines a controlled second phase that is the strength win — same “precipitation” word as chem-for-linguists §4, but the useful precipitate is γ′, not the corrosion-liability β of AA5083.
1. Chem-for-linguists checklist (§8) — filled
1. What is the inherent weakness of the pure / base form?
Pure / dilute-Ni lacks useful high-T creep strength: dislocationsLine defect enabling plastic slip at realistic stresses; edge vs screw are the two classic geometries. climb/glide around sparse obstacles as T rises. Separately, oxidation resistance at turbine temperatures needs enough Cr and/or Al (and often coatings). Design goal: raise elevated-T strength via a dense, coherent γ′ array while keeping ductility, processability, and environmental resistance acceptable for the duty (disk vs blade differ).
2. Which obstacle mechanism is doing the work?
Primary: coherent ordered γ′ precipitates — dislocations must cut (APB / order strengthening; weakly then strongly coupled pairs as size grows) or bypass (Orowan looping) once particles are coarse.
Secondary: solid-solution strengtheners in γ (Cr, Co, Mo, W, Re, …); carbides / GB segregants in polycrystalline alloys; in SX blades, rafting (directional coarsening under stress) can help or hurt creep depending on misfit and channel width.
Explicitly not: Mott-style impurity-band electronic doping as the design language for structural Ni superalloys.
3. What trade-offs are accepted?
- Higher γ′ fraction ↑ creep / strength ceiling, but ↓ ductility / forgeability / weldability if too high or wrongly sized.
- Refractory additions (Re, W, Mo, …) ↑ creep but promote brittle TCP phases (σ, μ, Laves, …) that deplete matrix strengtheners.
- Cr helps oxidation (Cr₂O₃) but modern high-Re SX alloys often cut Cr and rely more on Al₂O₃ + coatings — environment vs TCP trade.
- Unlike Cu–Ni, conductivity is not the headline metric; unlike AA5083, the useful second phase is strength, not a sensitization path — but wrong second phases (TCP, δ in 718-class, coarse overaged γ′) still fail the window.
4. How critical is processing vs nominal composition?
Extremely — first-class. Composition sets γ′ solvus, equilibrium volume fraction vs T, and TCP risk. Whether you get fine cuboidal/bimodal γ′ or coarse overaged particles depends on solution T (sub- vs super-solvus), cool rate, and multi-step aging. Service T–time–stress then drives coarsening / rafting / TCP. Composition alone does not “use up” the window.
5. Problem-driven or exploratory?
Problem-driven: keep a Ni host usable above ~0.5–0.7 Tm for creep + oxidation (chem-for-linguists’ jet-engine γ′ vignette), then stay inside the heat-treat and service envelope that delivers the intended γ/γ′ microstructure without TCP or uncontrolled overaging.
2. Explicit phase / diagram reading (diagram first)
2.1 What the Ni–Al / Ni–Al–Ti picture is telling you
Engineering reading starts from Ni-rich γ (FCC solid solutionSolute atoms dissolved into the host lattice (substitutional or interstitial) without a separate precipitate phase.) + ordered γ′ Ni₃(Al,Ti) (L1₂; cube-cube coherent with γ when fine):
| Fact | Approximate figure / lore | Role in reading |
|---|---|---|
| Essential γ′-formers | Al and/or Ti, typically total ≲ ~10 at% in classic Bhadeshia pedagogy | Generates two-phase γ + γ′ equilibrium microstructure |
| γ′ stoichiometry | Ideal Ni₃(Al,Ti); real γ′ not strictly stoichiometric (Al/Ti site mixing; Nb, Ta, Hf partition into γ′) | Composition sets misfit, APB energy, solvus |
| γ′ fraction vs T | For fixed alloy chemistry, fγ′ decreases as T rises → approaches zero at the γ′ solvus | Why solution treatment can dissolve γ′, then aging re-precipitates it fine |
| Disk / lower-T alloys | Often ~0.2–0.4 γ′ volume fraction class (Bhadeshia: ~0.2 enough near ~750 °C / weldable class; forged PM disk alloys often ~37–43% in Thermo-Calc examples for René 65 / AD730 / N19) | Fatigue / strength at moderate T; subsolvus solution common to retain primary γ′ for grain control |
| Blade / SX alloys | Often ≳ 0.6 cuboidal γ′ (Bhadeshia TEM pedagogy; metal >~1000 °C class) | Creep at extreme T; supersolvus / high solution T to dissolve coarse as-cast γ′ |
| Polycrystalline disk solvus examples | Thermo-Calc / experiment class: René 65 ~1093 °C, AD730 ~1108 °C, N19 ~1138 °C (Masoumi et al. 2021 Metals); primary γ′ dissolves steeply in a ~50 °C window below solvus | Subsolvus vs supersolvus process choice |
| SX solution window | Often ~1240–1330 °C class (Bhadeshia) — between γ′ solvus and incipient-melting / solidus limits | Homogenize + dissolve remnant solidification γ′ / eutectic, then age |
| Alloy 718 note (contrast, not pure γ′) | Nb-bearing; primary strength often γ″ Ni₃Nb (+ some γ′); γ″ solvus lore ~~900–926 °C class | Same precipitation checklist logic; different precipitate crystallography |
Sources (primary / near-primary pedagogy): Bhadeshia Cambridge Nickel based superalloys (phase-trans.msm.cam.ac.uk) — γ/γ′ structures, solvus reading, heat-treat bimodality, rafting misfit, TCP, SX solution T; Masoumi et al. 2021 Metals 11:1921 (primary γ′ dissolution / solvus for René 65, AD730, N19); Semiatin et al. / IMMI precipitation-modeling lineage for PM disk γ′ solvus approach curves; Waspaloy cutting/Orowan size windows (e.g. Mater. Charact. 2024 review line).
Reading rule: mark composition and draw the γ′ solvus. Above the solvus (given time), γ′ dissolves into γ. Below it, γ+γ′ is allowed; volume fraction rises as T falls (until kinetics freeze). Solution + quench (+ controlled cool) sets a supersaturated / fine-precipitate starting state; aging inside the two-phase field grows the useful size distribution. This is the chem-for-linguists sequence: solutionize → quench/cool → age.
2.2 Solvus / volume-fraction window — not one number
| Process choice | Materials intent | Risk if wrong |
|---|---|---|
| Subsolvus solution | Keep some primary γ′ to pin grains (disk / fatigue-sensitive) | Incomplete dissolve of fine hardening γ′ if T/time low; or grain growth if too close to solvus too long |
| Supersolvus solution | Dissolve γ′ → coarse γ grains; maximize later secondary/tertiary γ′ control (creep-focused) | Grain-size jump; approach incipient melting if above solidus locally |
| Primary + secondary aging | Bimodal γ′: coarser from higher-T age + finer from lower-T age (Bhadeshia standard picture) | Wrong T–time → wrong size → wrong cutting/Orowan balance |
| Service hold | γ′ should stay fine enough; rafting may be designed-in or tolerated | Overaging / Ostwald ripening; TCP; raft softening if channels widen |
One-sentence design reading: for Ni–γ′ you pick γ′-former chemistry and a solvus-relative heat-treat path, then defend that microstructure against service coarsening — not only a low-T solvus line (Al–Mg) or a conductivity curve (Cu–Ni) or a TTT/Ms map (Fe–C).
2.3 Host–solute site type vs prior checklists
| Host–solute story | Site / phase role | Design consequence |
|---|---|---|
| Al/Ti in Ni → γ′ | Substitutional formers of ordered precipitate (Ni₃X) | Strength from precipitate volume fraction + size, not from dissolved soluteIntentional minority species dissolved in the host (alloying addition). alone |
| Mg in Al | Substitutional SSS; β is usually a failure phase | Stay single-phase α for strength+corrosion |
| Ni in Cu | Substitutional complete SSS | No solvus ejecting Ni second phase |
| C in Fe | Interstitial; Fe₃C / martensite paths | Transformation / quench metastability |
3. Goal-dependent windows — name the mechanisms
“Useful window” is not one number. Name the goal first:
| Goal | Useful regime (materials) | Mechanism to name |
|---|---|---|
| High-T creep strength | High fγ′ (blade/SX often ≳0.6); controlled cuboids; sometimes negative misfit → rafting that blocks climb | Order/APB cutting; Orowan in channels; raft geometry vs channel width |
| Disk strength / fatigue | Moderate fγ′; fine secondary/tertiary γ′; often subsolvus grain control | Same cutting/Orowan map at lower T; GB carbides / clean PM processing |
| Oxidation / hot corrosion | Enough Cr and/or Al for protective Cr₂O₃ / α-Al₂O₃; coatings on many blades | Scale-forming chemistry — orthogonal to “more γ′ = better,” and can conflict with TCP/Re design |
| Processability (forge / weld) | Lower γ′ fraction / slower precipitation kinetics (Bhadeshia: ~0.2 class for lower-T weldable alloys) | Avoid unworkable hardness from premature γ′ |
Cutting vs Orowan (name it when teaching size): in Waspaloy-class γ′ studies, weakly coupled cutting for fine particles, strongly coupled cutting at intermediate radii, Orowan bypass when particles are coarse (order-of-magnitude: ~r ≲ 18 nm / ~18–98 nm / ~r ≳ 98 nm in one 2024 Waspaloy review — treat as alloy-specific illustration, not a universal constant).
Rafting (extreme T / stress): directional coarsening of γ′ under creep; misfit sign (Al/Ti ratio, Re partitioning into γ) sets raft orientation. Can reduce creep rate (climb blocked across rafts) or soften if γ channels widen and Orowan stress drops (crystal-plasticity / phase-field review lineage).
4. What “over” means — not one physics
Carry the Al–Mg / Cu–Ni / Fe–C lesson: “too much” is host- and goal-dependent. For Ni–γ′:
| Overrun mode | What goes wrong | Physics family |
|---|---|---|
| Coarsening / Ostwald ripening | γ′ grows; spacing ↑; cutting → Orowan; hardness/creep ↓ (overaging) | Interface-energy-driven ripening (slowed by low γ/γ′ energy when coherent) |
| Service rafting gone wrong | Topological inversion / wide soft γ channels | Stress + misfit + diffusion at extreme T |
| TCP phases (σ, μ, Laves, P, R, …) | Brittle particles; crack starters; deplete Re/W/Mo/Cr from γ | Refractory overload / phase stability |
| Too much γ′ (composition) | Ductility / toughness / forge–weld collapse; hard to solutionize without melting | Phase-fraction / process window |
| Wrong second phases (718-class) | δ / Laves / uncontrolled γ″→δ at elevated T | Nb-bearing alloy family (related checklist, different precipitate) |
| Under-solution / under-age | Coarse remnant γ′ or soft under-precipitated γ | Process miss — “under” on the heat-treat axis |
Honest split: none of these is a Mott MIT, none is AA5083 GB-β sensitization as the intended strength story, none is Cu–Ni Nordheim conductivity collapse, none is Fe–C martensite quench cracking. Same Bridge A count mnemonic only at the pedagogical layer (§9).
Under (for completeness): too little Al+Ti (or wrong aging) → soft γ-rich microstructure; miss creep / strength target — the dilute end of the same window.
5. Metastability / kinetics — first-class
| Step | State | Equilibrium? |
|---|---|---|
| Solution (sub- or super-solvus) | γ′ partially or fully dissolved in γ | Approaching high-T equilibrium if held long enough |
| Cool / quench | Supersaturated γ ± fine cooling γ′ (secondary) | Path-dependent; not a single equilibrium snapshot |
| Primary age (higher T in γ+γ′ field) | Coarser γ′ population | Controlled approach toward equilibrium fraction at that T |
| Secondary / tertiary age | Finer γ′; bimodal distributions common | Same — lower-T fraction increase |
| Service | Coarsening, rafting, possible TCP, Al depletion under oxide | Time–temperature–stress relaxation of the useful metastable/fine state |
Design rule (repeat from solubility-windows depth note): if the useful state is a fine precipitate distribution, schedule the relaxation risk explicitly (aging recipe; overtemp limits; coating + Al reservoir; TCP-safe chemistry). Service overaging is the Ni analogue of Al–Mg sensitization kinetics and Fe–C temper/service aging — different phases, same “useful state is not forever” lesson.
6. Vocabulary hygiene
| Prefer | Avoid for structural Ni superalloys |
|---|---|
| γ′-formers / Al–Ti alloying; precipitation hardening | “Dopant” / “doped Ni” (unless electronic intent is explicit) |
| Precipitate volume fraction fγ′ vs solute still dissolved in γ | Collapsing “amount of Al” into one number without saying dissolved vs precipitated |
| Cutting / APB / Orowan / rafting / TCP | Equating γ′ with linguistic arity or calling TCP an “adjunct” |
| Precipitation hardening ≠ electronic doping | Using “doped” because both put foreign atoms in a host |
Chem-for-linguists already splits alloying / doping / intercalation (§5) and lists precipitation hardening (§4) with the Ni γ′ jet-engine vignette. This checklist is that vignette expanded to solvus discipline.
Key pedagogy sentence: precipitation hardening ≠ electronic doping; solute concentration ≠ precipitate volume fraction (most of the Al/Ti inventory may sit inside γ′ particles, not as random γ solute).
7. Bridge A add-on checklist (depth note §6) — filled
-
Where is the solvus / solidus / critical boundary at process and service T?
Read γ′ solvus vs composition; mark sub- vs super-solvus solution; stay below incipient melting; then read service T against coarsening/TCP maps — not only the binary Ni–Al line. -
Intended mechanism?
Name it: coherent γ′ precipitation hardening (cutting/Orowan; optional rafting), plus SSS and oxidation chemistry. Do not call structural Ni–γ′ “electronic doping of nickel.” -
What fails first past the window?
Goal-dependent (§3–§4): overaging, TCP, ductility loss at high fγ′, oxidation if Cr/Al wrong, process melting — pick the failure that matches the named goal. -
Metastability?
Yes — central for the useful fine γ′ state. Aging builds it; service T–time–stress relaxes it (coarsening/rafting/TCP). -
Only then — SPECULATIVE Bridge A mnemonic
See §9. Never invert: do not pick Al+Ti% or age T from a linguistic arity table.
8. Under / useful / over — materials only (no linguistics yet)
| Zone | Ni–γ′ / superalloy reading (creep-first framing example) |
|---|---|
| Under | Too little γ′-former and/or under-aged: soft γ; sparse obstacles; miss creep / yield target |
| Useful window | Goal-relative: e.g. high-fγ′ cuboids + controlled rafting for SX blades; moderate fγ′ + subsolvus grain control for disks — always tied to solvus-relative heat treatment and oxidation chemistry |
| Over / wrong regime | Overaged coarse γ′; TCP from refractory overload; fγ′ so high ductility/processability collapses; or solution T that incipient-melts |
SPECULATIVE Cross-domain section. Open after the materials.
9. SPECULATIVE Bridge A overlay (supporting only)
Everything in this section is pedagogical analogy. It does not make doping × θ-roles a joint field.
| Materials fact | SPECULATIVE Bridge A reading |
|---|---|
| Useful γ′ fraction + age schedule for a named duty | Successful “saturation” of the design configuration |
| Under-alloyed / under-aged soft γ | Under-filling relative to the intended property configuration |
| Overaging / TCP / ductility collapse at excess formers | Overrun: chemistry still “fits” a phase diagram field, but leaves the useful property / phase cast |
| Continuous wt% + continuous T–time–stress | Same asymmetry as prior hosts: composition is continuous; verb arity is typically discrete — do not force integer slots onto Al+Ti% or fγ′ |
| Multiple distinct “over” physics | Bridge A’s count ladder is a memory peg; Ni–γ′ trains that “over” includes ripening kinetics and wrong second phases, not one solvus corrosion story |
Earn: teaches intentional precipitation windows (contrast Al–Mg, where β is usually unwanted); expands the host set with a high-T creep / oxidation peg.
Collapse: if γ′ cutting is equated with θ-saturation; if TCP is called an adjunct; if fγ′ is read off an arity table; if Navajo morphological typing is treated as evidence for this count story (typing stays parallel).
Explicit asymmetries (keep on the whiteboard): - Linguistics: often categorical well-formedness; Ni–γ′: graded optima + solvus-relative HT + service kinetics. - Continuous composition / fraction ≠ discrete lexical arity. - “Precipitate participants” are not θ-role fillers — metaphor only.
10. Contrast table — Ni–γ′ vs Al–Mg vs Cu–Ni vs Fe–C
| Ni–γ′ (this note) | Al–Mg AA5083 | Cu–Ni | Fe–C | |
|---|---|---|---|---|
| Solute / phase role | Substitutional γ′-formers → ordered precipitate | Substitutional Mg SSS; β unwanted | Substitutional Ni complete SSS | Interstitial C |
| Diagram family | γ / γ′ solvus; fγ′(T) ↓ toward solvus | Limited solubility; solvus + β | Isomorphous complete SSS | Eutectoid Fe–Fe₃C; α≪γ C solubility |
| Headline “window” metric | γ′ size + volume fraction + solvus-relative HT; oxidation chemistry | Solvus + service T–time + DoS | Conductivity / resistivity curves | Transformation path (pearlite / M / temper) |
| First “over” (typical) | Overaging / Ostwald; TCP; excess fγ′ ductility loss | GB β sensitization (IGC) | Property-curve overrun (Nordheim-family) | Cementite networks; brittle M; RA / TME |
| Useful second phase? | Yes — γ′ is the strength win | No — β is failure mode | No Ni second phase in binary | Cementite / tempered carbides — morphology-dependent |
| Metastability of useful state | Central (fine γ′; service coarsening/rafting) | Useful Mg SSS often supersaturated | Binary α equilibrium at all Ni% | Central (quench M, RA, temper) |
| Bridge A second-phase peg | Strong (wanted γ′ vs unwanted TCP) | Strong (unwanted β) | Weak / absent for binary Ni | Strong for cementite morphology + transformation peg |
| Vocabulary | γ′-formers / alloying; avoid “dopant” | Solute; avoid “doped Al” | Solute; avoid “doped Cu” | Solute / alloying; avoid “dopant” |
Pedagogy takeaway: four hosts, four “over” families — phase/corrosion (Al–Mg), property-curve (Cu–Ni), phase-morphology + quench metastability (Fe–C), precipitation-size/fraction + TCP/overaging (Ni–γ′). Bridge A’s under/useful/over ladder is only hung after the mechanism is named.
11. What this walkthrough trains you to do next
For any new host/solute pair:
- Classify whether the useful obstacle is dissolved solute, intentional precipitate, or transformation product.
- Open / sketch the relevant diagram; mark solvus (or TTT/Ms) and process vs service T.
- Name the mechanism (SSS / γ′ cutting–Orowan / pearlite / martensite / electronic doping / …).
- Name the metric that defines the useful window (fγ′+size vs DoS vs conductivity vs hardenability).
- Name the first failure past that window — expect plural modes in superalloys.
- Ask whether the useful state is metastable (yes for fine γ′ under service).
- Only then, if useful for memory, hang the SPECULATIVE Bridge A count peg.
Stacked with Al–Mg, Cu–Ni, and Fe–C: you now have four REAL host pegs on disk — sensitization, conductivity, interstitial-C transformation/metastability, and γ′ precipitation windows — without claiming any is linguistics.
Queued later (CONCLUSIONS §7, optional): process metastability case study as Bridge A’s kinetics half (Al–Mg / Fe–C / Ni–γ′ already supply three kinetics stories); Grant source-PDF drops.
12. Sources consulted (2026-09-15 note)
| Source | Role |
|---|---|
| Bhadeshia, H.K.D.H. — Nickel based superalloys (Cambridge phase-transformations site) | REAL: γ/γ′ L1₂; Al/Ti ≲10 at%; fγ′(T); solution+double age; rafting/misfit; TCP σ/μ; SX solution ~1240–1330 °C; oxidation Cr/Al; disk vs blade fractions |
| Masoumi et al. 2021 Metals 11:1921 — primary γ′ dissolution (René 65, AD730, N19) | Near-primary: Thermo-Calc solvus ~1093 / 1108 / 1138 °C; RT fγ′ ~37–43%; ~50 °C subsolvus dissolution window |
| Semiatin et al. IMMI precipitation / PM disk γ′ modeling lineage | Engineering solvus approach curves; primary/secondary/tertiary γ′ vocabulary |
| Waspaloy precipitation-hardening mechanism reviews (e.g. Mater. Charact. 2024 line) | Cutting (weak/strong couple) vs Orowan size regimes illustration |
| TCP / thermal-exposure reviews (e.g. Crystals / MST TCP overview lineage; PMC10003985) | Overaging, rafting, refractory-driven TCP depletion of γ strengtheners |
| Project-internal: Conclusions §7; Al / Cu / Fe–C checklists; Solubility windows; Chem for linguists §4–§8 | Stack consistency; precipitation vignette expansion; Bridge A lock |
v0 — 2026-09-15 continue-research. Real metallurgy walkthrough; Bridge A flagged SPECULATIVE. No joint field.
Corpus note: worked-ni-gamma-prime-checklist-v0.md. Materials first; Bridge A peg last.