Sixteen host checklists
Path C, in the order of the conclusions addendum. Every checklist uses the same discipline: diagram, mechanism, failure past the window, metastability, then a SPECULATIVE Bridge A peg.
Prefer solute / alloying for percent-level solid solution. Reserve dopant for dilute electronic intent (Si, GaN:Mg, oxide). Say intercalant for channel and gap charge transfer. For NMC, papers say doping; the meter is structural stability, not carrier density.
| # | Host | Diagram / lattice | First “over” |
|---|---|---|---|
| 1 | Al–Mg | Limited solvus; FCC Al + subst. Mg | GB β / sensitization (IGC) |
| 2 | Cu–Ni | Isomorphous complete SSS | Conductivity / TCR property curves |
| 3 | Fe–C | Eutectoid Fe–Fe₃C; interstitial C | Cementite networks / brittle as-quenched M / temper–RA |
| 4 | Ni–γ′ | γ/γ′ solvus; wanted precipitate | Overaging / rafting gone wrong / TCP |
| 5 | Mg host | HCP; AZ/AM/ZK (+ RE) | Brittle IMCs; galvanic β; creep; ignition; anisotropy miss |
| 6 | Ti host | HCP α / BCC β; β-transus; Ti-6Al-4V | α-case; O/H embrittlement; ω; β flecks; overaging |
| 7 | Oxide electronic | Wide-gap oxide + subst. metal + V_O | Recombination centers; μ collapse; secondary oxides; vacancy compensation |
| 8 | CNT / graphene | sp² framework + guest in channels/gaps | Moisture dedoping; diffusion blur; junction R; no band gap for switching |
| 9 | GaN:Mg | Wurtzite GaN + Mg_Ga acceptor (+ H) | Self-compensation; PIDs; μ/optical loss; failed activation |
| 10 | Si:P/As/B | Diamond Si + shallow subst. donors (P, As) / acceptors (B) | Impurity band / Mott; clustering; μ collapse; compensation |
| 11 | NMC:Mg cathode | Layered oxide + dilute Mg/Al/Nb lattice stabilizers | Inactive capacity; Li-path blocking; secondary phases; thermal still fails if cutoff insane |
| 12 | Cantor HEA | Equiatomic FCC MPEA; five co-principal alloying elements | Cryogenic nanotwinning / TWIP; composition or long-anneal phase drift |
| 13 | TWIP Fe–Mn | FCC γ Fe–Mn–C(–Al–Si); SFE bands (~15–30 wt% Mn) | Too-low SFE → TRIP/ε; too-high → no twin; H delayed fracture |
| 14 | Al–Li | FCC Al + Li (+Cu…); δ′ Al₃Li / T₁ Al₂CuLi | Anisotropy / toughness (planar slip) / SCC / overaging / melt Li loss |
| 15 | CoCrMo | Co-majority FCC γ (+ ε); ~28Cr–6Mo; F75/F1537; SIMT + M₂₃C₆ | Brittle carbide networks; Cr depletion; uncontrolled ε; fretting/MACC ions |
| 16 | Zr nuclear | HCP α service / BCC β process; Zircaloy / Zr–Nb; SPPs | Nodular/uniform corrosion; hydriding/DHC; LOCA breakaway; SPP fluence evolution; growth/bow |
Cross-cuts that compare hosts live under Bridge A: mechanism families, same-element Mg, H, Al, Ni, Mn, and Co, precipitation, SFE, HCP, allotropy, solid solution, the alloying–doping–intercalation triangle, plural “over” modes, and clocks.